Events

- This event has passed.
Aluminum Casting Defects: Root Cause Analysis & Corrective Action
January 25 @ 8:30 am - 3:00 pm
Class material includes:
- Root cause analysis and corrective actions for common aluminum casting defects
- Overview of the latest technologies and analysis methods for performing defect root cause analysis
- Case studies using MAGMASOFT® Autonomous Engineering to reduce scrap and rework
This is a free training event and will include lunch with 20 seats available on a first-come, first-serve basis.